  • in reply to: Lincoln TIG welds have dark spots #69889
    Participant
    Heather JonesHeather Jones

      Dark spots comes from poor gas coverage or prep, Check for leaks at 20 CFH argon, My Lincoln TIG had same issues, Clean steel with alcohol before welding, Set AC balance to 65% for control, Use 2% lanthanated tungsten for stability, Use 15 CFH argon to avoid turbulence, Sharpen tungsten fine, Ensure clean connections, Use wire brush for prep.