What causes miller 252 welder porosity? why’s my Miller 252 welder leaving porous welds with 0.035-inch mig wire at 20 CFH argon? welds look bad, any ideas?
- 3
- 6 months, 2 weeks ago
-
Why Does Welder Display Flicker? i am confused cause my Lincoln PowerMIG 260 display flickers on start at 24 volts, And the screen dims. Any ideas?
- 4
- 7 months, 1 week ago
-
welding helmet lens scratches bad my Hobart Impact lense scratches bad, hard to see. Any solution?
- 5
- 8 months ago
-
welding brushed stainless steel scratches My brushed stainless steel scratches during welding cleanup using a stainless brush on TIG welds, welds looks marked. Any fixes?
- 4
- 9 months, 2 weeks ago
-
Getting odd miller 120v stick welder on stainless — electrode sticking Hi guys, my Miller 120v stick on stainless sticks, cleaned with acetone, tweaked CFH 15 to 25. Can you give me a solution to this?