  • in reply to: YesWelder TIG welds look wierd #69822
    Participant
    Dana HerreraDana Herrera

      Weird welds comes from poor prep or settings, Clean steel with acetone before welding, My YesWelder had same issue, Use 120 amps for 1/8-inch steel, Set AC balance to 65%, Check tungsten sharpness, Use 25 CFH argon, Ensure clean joint fit-up.