Lincoln welder welds have porous spots

Viewing 4 reply threads
  • Author
    Posts
    • #69953
      Participant
      Danielle Richards

        This is driving me nuts cause my Lincoln PowerMIG 260 welds has porous spots on steel, Using 0.035-inch wire at 24V, and welds shows bubbles. How i can avoid this problem?

      • #69955
        Moderator
        Aaron Austin

          Porosity comes from dirty steel or gas issues, Clean with acetone thorough before welding, My PowerMIG 260 had bubbly welds too, Use 25 CFH argon for better coverage, Check gas hose for leaks, Set wire speed to 240 ipm for consistency, Use 7018 electrodes for cleaner welds, Ensure clean joint fit-up, Use wire brush for prep, Verify regulator settings.

        • #69956
          Participant
          Jasmine Foley

            bubbly welds comes from dirty surfaces, Degrease with alcohol thorough before welding, My Lincoln welds clean now, Check gas flow for consistency.

          • #69957
            Participant
            Lisa Allen

              Increase gas flow to reduce porosity, it helps.

            • #69958
              Participant
              Jessica Martinez

                Use fresh wire to avoid bubbles, My Lincoln got better after switching, Check connections.

            Viewing 4 reply threads