Hobart 190 leaves porous welds

Viewing 2 reply threads
  • Author
    Posts
    • #69472
      Participant
      Richard Myers

        i’m a little bit confused cause my Hobart 190 leaves porous welds on aluminum with 0.035-inch mig wire at 20 CFH argon, welds look bad. How i can avoid this problem?

      • #69474
        Moderator
        Chad King

          Check for gas leaks on your Hobart 190, use 25 CFH argon, fixes porosity.

        • #69475
          Participant
          William Daniels

            Clean aluminum with alchohol before welding, dirty metal causes porosity, use fresh mig wire.

        Viewing 2 reply threads